17Cr2Ni2Mo圆钢在经过淬火的淬火温度时,即1040℃时,它的切削性、磨削性会较好,且电加工变质层残余应力小,残余奥氏体极少,碳化物细小。
17Cr2Ni2Mo圆钢的热处理过程,若发现是精密冲模、修整模、冷轧辊轮等工模具时,应采用低温回火工艺。
因为低温回火工艺可以使模具工作零件获得高硬度、高韧性、耐磨性好、强度高,并且还可以有效延长模具寿命,以此来防止模具出现过度磨损、变形、开裂等早期失效现象。